Viewed 2638 Times

Question:

Why does NACE MR0175 / ISO 15156, Part 3 specifically demand age-hardening although age-hardening typically increases the hardness of UNS R30003? Is this because problems were reported when the material was not age-hardened, because data is only available for age-hardened material, or another reason?

Answer:

In Table A.39 the cold worked + age hardened condition of UNS R30003 was the only condition originally balloted and accepted.

This question is in relation to NACE MR0175/ISO 15156-3 Table A.39

Reference: ISO 15156 Maintenance Panel Inquiry #2009-05

Contact us to discuss the UNS R30003 NACE MR0175 in the latest revision.

 

With a wealth of experience in the oil and gas industry, we provide independent materials and corrosion consultancy to help companies reduce risk, save money and apply best practice in their oil and gas businesses.

Find out more by getting in touch – you’ll get an answer from a qualified, experienced materials engineer every time.

 

USA toll-free

 

US: 877-399-1010 (toll free)
UK: +44(0)1144000850

66 Eldon St
Sheffield
S1 4GT
United Kingdom

 

Was this answer helpful ? Yes / No